The Nd : YAG laser welding was used to join the TiNi shape memory alloy and AISI304 stainless steel wires. The microstructural features of the dissimilar material joint were analyzed. The tensile and hardness tests were carried out to examine the mechanical properties and microhardness distribution of the welded joint. The results show that the joint has the non-homogeneous microstructure and element distribution. The brittle phases such as Fe2 Ti , Fe Ti , Cr2 Ti , Ti3 Ni4, Feo 2 Ni4.s Ti5 and TiN mainly segregate in rich Ti region of fusion zone. The laser-welded joint has the tensile strength of 298 MPa with the elongation of 3.72 % and exhibits the brittle fracture features on the fracture surfaces. The reasons for low joint strength were discussed in this investigation.